[資源]
Ductile crystalline–amorphous nanolaminates
|
||
|
Ductile crystalline–amorphous nanolaminates Yinmin Wang*†‡, Ju Li§, Alex V. Hamza*†, and Troy W. Barbee, Jr.† *Nanoscale Synthesis and Characterization Laboratory, †Chemistry, Materials, and Life Sciences Directorate, Lawrence Livermore National Laboratory, Livermore, CA 94550; and §Department of Materials Science and Engineering, Ohio State University, Columbus, OH 43210 Edited by William D. Nix, Stanford University, Stanford, CA, and approved May 25, 2007 (received for review March 14, 2007) (美國(guó)科學(xué)院院刊) It is known that the room-temperature plastic deformation of bulk metallic glasses is compromised by strain softening and shear localization, resulting in near-zero tensile ductility. The incorporation of metallic glasses into engineering materials, therefore, is often accompanied by complete brittleness or an apparent loss of useful tensile ductility. Here we report the observation of an exceptional tensile ductility in crystalline copper/copper–zirconium glass nanolaminates. These nanocrystalline–amorphous nanolaminates exhibit a high flow stress of 1.09 0.02 GPa, a nearly elastic-perfectly plastic behavior without necking, and a tensile elongation to failure of 13.8 1.7%, which is six to eight times higher than that typically observed in conventional crystalline– crystalline nanolaminates (<2%) and most other nanocrystalline materials. Transmission electron microscopy and atomistic simulations demonstrate that shear banding instability no longer afflicts the 5- to 10-nm-thick nanolaminate glassy layers during tensile deformation, which also act as high-capacity sinks for dislocations, enabling absorption of free volume and free energy transported by the dislocations; the amorphous–crystal interfaces exhibit unique inelastic shear (slip) transfer characteristics, fundamentally different from those of grain boundaries. Nanoscale metallic glass layers therefore may offer great benefits in engineering the plasticity of crystalline materials and opening new avenues for improving their strength and ductility. metallic glass /size-dependent plasticity / nanocrystalline materials /amorphous–crystalline interface / tensile ductility |
| 最具人氣熱帖推薦 [查看全部] | 作者 | 回/看 | 最后發(fā)表 | |
|---|---|---|---|---|
|
[考研] 石河子大學(xué)(211、雙一流)碩博研究生長(zhǎng)期招生公告 +3 | 李子目 2026-03-22 | 3/150 |
|
|---|---|---|---|---|
|
[考研] 北科281學(xué)碩材料求調(diào)劑 +6 | tcxiaoxx 2026-03-20 | 6/300 |
|
|
[考研] 287求調(diào)劑 +8 | 晨昏線與星海 2026-03-19 | 9/450 |
|
|
[考研] 考研調(diào)劑 +4 | 來好運(yùn)來來來 2026-03-21 | 4/200 |
|
|
[考研] 085600材料與化工306 +4 | z1z2z3879 2026-03-21 | 4/200 |
|
|
[考研] 286分人工智能專業(yè)請(qǐng)求調(diào)劑愿意跨考! +4 | lemonzzn 2026-03-17 | 8/400 |
|
|
[考研] 化學(xué)調(diào)劑 +5 | yzysaa 2026-03-21 | 5/250 |
|
|
[考研] 278求調(diào)劑 +9 | 煙火先于春 2026-03-17 | 9/450 |
|
|
[考研] 求調(diào)劑 +3 | .m.. 2026-03-21 | 4/200 |
|
|
[考研] 0805材料320求調(diào)劑 +3 | 深海物語 2026-03-20 | 3/150 |
|
|
[考研] 332求調(diào)劑 +4 | ydfyh 2026-03-17 | 4/200 |
|
|
[考研] 274求調(diào)劑 +10 | S.H1 2026-03-18 | 10/500 |
|
|
[考研] 261求B區(qū)調(diào)劑,科研經(jīng)歷豐富 +3 | 牛奶很忙 2026-03-20 | 4/200 |
|
|
[考研] 工科材料085601 279求調(diào)劑 +7 | 困于星晨 2026-03-17 | 9/450 |
|
|
[考研] 08工學(xué)調(diào)劑 +5 | 用戶573181 2026-03-20 | 5/250 |
|
|
[考研] 0703化學(xué)調(diào)劑 +5 | pupcoco 2026-03-17 | 8/400 |
|
|
[考研] 材料考研調(diào)劑 +3 | xwt。 2026-03-19 | 3/150 |
|
|
[考研] 277調(diào)劑 +5 | 自由煎餅果子 2026-03-16 | 6/300 |
|
|
[碩博家園] 湖北工業(yè)大學(xué) 生命科學(xué)與健康學(xué)院-課題組招收2026級(jí)食品/生物方向碩士 +3 | 1喜春8 2026-03-17 | 5/250 |
|
|
[考研]
|
zhouzhen654 2026-03-16 | 3/150 |
|